01 / THE TOOL COLLECTION

Polishing Tools

Explore diamond tooling by product, material and application. Confirm standard specifications and customization in the catalog.

Matching tools 2 / 23
Concept still life of cutting, grinding and polishing tools
Concept still life of cutting, grinding and polishing toolsCONCEPT VISUAL

Diamond polishing pads: Formulated with high-grade micro-diamond powder and temperature-resistant polymer resins. Choose 7-step dry honeycomb pads for on-site fabrication, or white-resin wet pads to prevent dark staining on white marble and sintered stone.

Not sure which tool fits your job? Try the 3-Step Wizard

Filter preliminary candidates by material and machine type, then confirm fitment and job conditions

Diamond Tool Models & Specifications

Formulated to match workpiece hardness, machine power and operating linear speed.

Material:
Cooling:
BUYING GUIDE · TECHNICAL SELECTION

How Do You Achieve High Gloss on Sintered Stone and Granite Without Burning the Surface?

High gloss requires progressive scratch refinement without excessive heat generation. Transitioning properly from coarse to fine grits prevents surface hazing.

Polishing Pad Technology Comparison

Pad ConstructionRecommended SubstratesGrit SequenceCooling & Operation Requirements
Dry Honeycomb PadSintered slabs, granite, quartz countertopsQZ-PP-DR07, 100mm (4 inch), 50# to 3000#No water needed; maintain RPM under 4,500 to avoid burn
Engineered Wet Polishing PadWhite marble, limestone, terrazzo, graniteQZ-PP-WT06, 80mm to 125mm, white resin matrixContinuous water flood, prevents stone discoloration

Key Polishing Terminology Explained

Grit Progression Rule

Each diamond grit stage is formulated to remove the scratch pattern left by the preceding grit. Skipping a grit (e.g. going from 100# directly to 400#) leaves deep micro-fissures that permanently dull final gloss.

Thermal Resin Smear

When dry pads run at excessive speeds or dry-rubbed without relief, friction heat exceeds the resin melting point, smearing burnt polymer into stone pores. High-Tg resin matrices prevent this defect.

Diamond Polishing Pad FAQs

Q1.Why does white marble or white sintered stone turn gray or yellow after edge polishing?

Discoloration is caused by dark resin binders in cheaper pads melting into stone pores under heat. Always use white or light-colored resin pads (such as QZ-PP-WT06) for pale natural stones and sintered slabs.

Q2.What is the optimal angle grinder speed for flexible dry polishing pads?

Optimal speed is 2,000 to 4,000 RPM. Standard single-speed angle grinders running at 11,000 RPM run far too fast, rapidly vaporizing resin, burning the pad, and ruining the stone surface. Always use variable-speed polishers.